Surface Field & Pull Force Calculator

Enter a magnet's shape, size and grade to estimate its surface field (mT / gauss) and pull force range.

  • Free
  • No sign-up
  • Engineer check on request

1Magnet

Shape

Top view (pole face)

Cross-section

T is the thickness along the magnetisation (arrow, S→N inside the magnet); D, L × W or OD / ID are across it. Labels show the values entered.

2Measurement & working temperature

3Steel it sticks to

Surface field 410–423 mT ≈ 4,105–4,232 Gs|Pull force 16.3–26.1 N

Surface field 410–423 mT; Pull force 16.3–26.1 N

Surface field

410–423 mT

≈ 4,105–4,232 Gs

Centre of the pole face · includes the industry 0.9 factor — enter the real measuring distance · at 20 °C

Pull force

16.3–26.1 N

≈ 1.67–2.66 kgf

Pull-off force perpendicular to flat mild steel (upper end = best case) · at 20 °C

On a vertical steel surface the sliding hold is only ~20–30 % of this even when clean, dry and in full contact — much less with oil, paint or vibration; confirm by test with a safety factor.

Estimates (theory with an empirical 0.9 factor on surface field) for preliminary selection only. Temperature is applied as a reversible Br change; the grade's max working temperature (80 °C) is a catalogue value and must be checked against the magnet's working point (thin magnets demagnetise at lower temperatures). Pull assumes clean, flat mild steel of the thickness entered; plate saturation is a simplified estimate.

Need measured data? Contact our engineers

Field around the magnet

Field lines and |B| — section through the axis (at maximum Br)
01 T

Ideal uniformly magnetised magnet, N face up. Shading is flux density on a square-root scale (so the weak fringe field stays visible); lines are field lines. The dot marks the measuring point.

Field against measuring distance
011422934345703.757.511.315Distance from pole face, mmmT

0 mm · 410–423 mT

Same basis as the result above (industry 0.9 factor included); band = grade Br min–max at the working temperature.

Surface field and pull force of common NdFeB magnet sizes

Estimated surface field at the centre of the pole face and perpendicular pull force for common NdFeB discs, blocks and rings at 20 °C, as ranges over each grade's remanence (N35, N42, N52). Sizes in mm; the last figure is the thickness along the magnetisation.

Size (mm)N35N42N52
Ø5 × 2332–346 mT · 0.304–0.495 kgf363–374 mT · 0.363–0.579 kgf402–416 mT · 0.446–0.717 kgf
Ø10 × 3273–285 mT · 0.992–1.62 kgf299–308 mT · 1.19–1.89 kgf331–343 mT · 1.46–2.34 kgf
Ø10 × 5375–391 mT · 1.39–2.27 kgf410–423 mT · 1.67–2.66 kgf455–471 mT · 2.05–3.29 kgf
Ø20 × 5237–248 mT · 3.44–5.6 kgf260–268 mT · 4.11–6.55 kgf288–298 mT · 5.05–8.11 kgf
Ø20 × 10375–391 mT · 5.58–9.09 kgf410–423 mT · 6.67–10.6 kgf455–471 mT · 8.19–13.2 kgf
Ø30 × 10295–307 mT · 9.65–15.7 kgf322–332 mT · 11.5–18.4 kgf357–369 mT · 14.2–22.8 kgf
20 × 10 × 5300–312 mT · 2.79–4.55 kgf327–338 mT · 3.34–5.32 kgf363–376 mT · 4.1–6.59 kgf
40 × 20 × 10300–312 mT · 11.2–18.2 kgf327–338 mT · 13.3–21.3 kgf363–376 mT · 16.4–26.3 kgf
Ø20/Ø10 × 5367–383 mT · 3.82–6.23 kgf402–414 mT · 4.57–7.29 kgf445–461 mT · 5.62–9.02 kgf

Field includes the industry 0.9 factor; a ring is measured over the middle of its wall. Pull is in kilograms-force (1 kgf ≈ 9.8 N), as an empirical range for the model conditions (thick steel, no gap): the top is clean, flat mild steel (best case), the bottom a cautious estimate — neither is a guarantee. Paint, tape or plating act as a gap and thin steel also cuts the pull, so real values can fall below the bottom — enter them as the air gap in the calculator above, and confirm by test.

How the calculator works

  • Field: a uniformly magnetised body is modelled as surface charge on its two pole faces (μr ≈ 1), giving Bz at the face centre or at the measuring distance; closed forms for discs and blocks, a ring is integrated over the middle of its wall.
  • Quoting convention: the field is quoted as theory × 0.9, the industry practice confirmed by AIC's engineers. It is a blanket quoting factor, not a probe-offset correction: enter the gaussmeter's Hall-element offset as the measuring distance, and confirm by measurement.
  • Pull: an ideal thick steel plate is replaced by the magnet's mirror image and the Maxwell stress is integrated over the whole plate (fringe flux included). That is an upper bound; real steel is never ideal, so the page shows 50–75 % of it as an empirical range (not a guarantee); paint, tape or plating must be entered separately as the air gap.
  • Thin plate saturates, and pull is derated by the flux the plate can carry; temperature corrects remanence reversibly only and does not check for irreversible demagnetisation.
  • For single axially magnetised discs, blocks and rings; multi-pole magnets, assemblies and steel-backed circuits need their own calculation.

FAQ

Why does my gaussmeter read lower than the calculator?

A gaussmeter's Hall element sits a little behind the probe tip, so it reads the field slightly away from the face; an off-centre probe also reads low. The result includes the 0.9 quoting factor, which does not stand in for the probe offset: enter the probe's real offset as the measuring distance before comparing — the larger the offset and the smaller or thinner the magnet, the lower the reading.

Why is pull force given as a range?

The model assumes infinitely thick, perfectly flat, ideal steel — an upper bound. Real steel is never ideal, so the page shows 50–75 % of the theoretical value as an empirical range: the top for clean thick steel, the bottom on the cautious side — neither a guarantee. Paint, tape or plating act as a gap: enter their thickness as the air gap; real values can fall below the range, so confirm by test.

How much pull is lost on thin steel or through paint?

Both an air gap and thin steel cut pull force markedly. Enter the gap (paint, tape, plastic) and the plate thickness in the calculator to see the derating; very thin plate is flagged as saturated.

How much will a magnet hold on a vertical steel surface?

On a vertical surface the magnet is held by friction. On clean, dry steel in full contact that is, as a rough rule, only about 20–30 % of the perpendicular pull-off force — much less with oil, paint, an uneven surface or vibration. Size hanging or anti-slip loads from the actual pull force and friction coefficient, with a safety factor, and confirm by test.

How does temperature affect field and pull?

NdFeB remanence falls reversibly with temperature (about −0.12 %/°C): field drops in proportion and pull roughly with the square. Too hot, it can also demagnetise irreversibly: a grade's maximum working temperature is a catalogue value at a typical working point, and a thin magnet or one under a strong opposing field can demagnetise below it — check the real working point; for heat choose H, SH, UH grades or SmCo.

AIC Engineering team · model and tables updated October 2026. Table values come from the same model as this page's calculator.